Sign In | Join Free | My insurersguide.com
China Danyang Kaixin Alloy Material Co., Ltd. logo
Danyang Kaixin Alloy Material Co., Ltd.
Danyang Kaixin Alloy Material Co., Ltd.
Verified Supplier

3 Years

Home > Inconel Alloy >

ASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy Nickel Alloy Wire

Danyang Kaixin Alloy Material Co., Ltd.
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

ASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy Nickel Alloy Wire

Brand Name : KAIXIN

Model Number : KX-Alloy IN P718

Certification : ISO9001:2015

Place of Origin : China

MOQ : 200KG

Price : To negotiate

Payment Terms : T/T, L/C

Supply Ability : 50~80 TONS per MONTH

Delivery Time : 45~60days

Packaging Details : Wooden Box, size as per guests' request

Shape : Wire,Strip,Rod,Pipe,Plate

Alloy Type : Nickel-based Superalloy

Raw Materials : NI Rem,CR18%,Co9% ,MO2.75%

Executive standard : ASTM

Delivery State : Soft State

Application : Used for disc, brake, fastener, blade and etc

Features : High temperature resistance

Size : Negotiable

Contact Now

KX Inconel 718 Plus Nickel Alloy Wire Round Bar Tube Steel Sheet Light Rod On Inconel Alloy

Product Description and Application

Inconel718 plus is a new type of nickel-based precipitation-hardened alloy, which is widely concerned at home and abroad because of its excellent comprehensive mechanical properties below 700°C, good thermal working and welding properties, suitable cost. At present, this material has been promoted and applied in several well-known aero-engine companies, which are used in disc parts, brakes, fasteners, blades and etc. In addition, Inconel718 Plus is also commonly used in copper extrusion mold.

Process Performance and Requirements

  • Product Fusion Process

Vacuum Induction Furnace(VIM) and Electroslag Remelting Furnace(ESR)

  • Product Chemical Composition

Element C Ni Cr Mo W Co Fe Nb Ti Al P B
Inconel718 plus 0.02 Rem 18 2.75 1 9 10 5.45 0.7 1.45 0.01 0.004

  • Product Physical Property

Density 8.25g/cm3
Melting Temperature Range 1260~1340℃

  • Product Mechanical Property

Hardness:

The hardness is about 20-30HRC after solid solution heat treatment and about 38-45HRC after annealing

  • Productive Process

ASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy Nickel Alloy Wire

  • Professional Customization

Cold-drawn Wire ¢0.3~¢18mm(Delivery in rolls or trays)
Hot-Rolling Wire ¢5.5~¢20mm(Delivery in rolls)
Strip thickness 0.1~4.5*width 6~350mm(Supply in rolls or straight strips)
Smooth Forged Rod on a Lathe

¢60~350mm,L800-2500mm

Hot-rolled Burnishing ¢20~80mm,L1000-5000mm
Cold Drawn and Burnishing ¢2.5~18mm,L1000-8000mm
Seamless Tube ¢1~275mm,wall thickness 0.2~30,L1000-8000mm

ASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy Nickel Alloy WireASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy Nickel Alloy WireASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy Nickel Alloy WireASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy Nickel Alloy WireASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy Nickel Alloy WireASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy Nickel Alloy WireASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy Nickel Alloy Wire


Product Tags:

ASTM Inconel Alloy

      

Round Inconel Alloy

      

Inconel 718 round bar

      
Cheap ASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy Nickel Alloy Wire for sale

ASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy Nickel Alloy Wire Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Danyang Kaixin Alloy Material Co., Ltd.
*Subject:
*Message:
Characters Remaining: (0/3000)