ASTM Standard Alloy 600 Inconel Alloy Nickel Based Deformed Superalloy And MO2.8-3.3%

Danyang Kaixin Alloy Material Co., Ltd.
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

ASTM Standard Alloy 600 Inconel Alloy Nickel Based Deformed Superalloy And MO2.8-3.3%

Brand Name : KAIXIN

Model Number : inconel 600

Place of Origin : China

Certification : ISO9001:2005

MOQ : 30kg

Price : 50-52 USD/kg

Packaging Details : wooden box

Delivery Time : 15-20 days

Payment Terms : T/T L/C

Supply Ability : 100000KG/MONTH

Delivery State : Sosoloid

Features : Fatigue Resistance, Radiation Resistance, Oxidation Resistance, Corrosion Resistance

Alloy Type : Nickel-based Deformed Superalloy

Application : Parts For Aero-engine, Nuclear Energy Industry And Petroleum Applications

Shape : Wire,Strip,Rod,Pipe,Plate

Executive standard : ASTM

Size : Negotiable

Raw Materials : NI50-55%, CR17-21%, NB4.75-5.5%, MO2.8-3.3%

Contact Now

ASTM Standard Alloy 600 Inconel Alloy Nickel-Based Deformed Superalloy And MO2.8-3.3%

Product Description:

Inconel 625 is a nickel-based deformed superalloy that has superior fatigue resistance, radiation resistance, oxidation resistance, and corrosion resistance. It is an ideal choice for parts that are used in aero-engine, nuclear energy industry, and petroleum applications. It is available in a variety of shapes such as wire, strip, rod, pipe, and plate, and the size can be customized according to the customer’s requirements. Inconel 625 is capable of withstanding extreme temperatures and high pressures. It also has excellent weldability and can be easily machined to the desired shape. It is an ideal material for components that require superior mechanical properties and corrosion resistance.

Features:

  • Product Name: Inconel Alloy
  • Raw Materials: NI50-55%, CR17-21%, NB4.75-5.5%, MO2.8-3.3%
  • Features:
    • Fatigue Resistance
    • Radiation Resistance
    • Oxidation Resistance
    • Corrosion Resistance
  • Alloy Type: Nickel-based Deformed Superalloy
  • Application: Parts For Aero-engine, Nuclear Energy Industry And Petroleum Applications
  • Shape: Wire,Strip,Rod,Pipe,Plate
  • Highlight:
    • Inconel 625, no 6625, AWSA5.14:2005 alloy 625

Technical Parameters:

Property Description
Alloy Type Nickel-based Deformed Superalloy
Features Fatigue Resistance, Radiation Resistance, Oxidation Resistance, Corrosion Resistance
Size Negotiable
Raw Materials NI50-55%, CR17-21%, NB4.75-5.5%, MO2.8-3.3%
Shape Wire,Strip,Rod,Pipe,Plate
Application Parts For Aero-engine, Nuclear Energy Industry And Petroleum Applications
Executive standard ASTM
Delivery State Solid
AWSA5.14:2005 alloy 625 Nr.2.4856

Applications:

Inconel Alloy, also known as UNS N06625 or Alloy 625, is a nickel-chromium-molybdenum alloy with high strength and excellent corrosion resistance. It is used in a variety of industrial applications, such as aircraft parts, chemical processing, power plants, and nuclear reactors. KAIXIN's Inconel 600 has been certified by ISO9001:2005 and its raw materials include NI50-55%, CR17-21%, NB4.75-5.5%, MO2.8-3.3%. The executive standard is ASTM and the delivery state is sosoloid. It is available in various shapes, such as wire, strip, rod, pipe, and plate. The size is negotiable and the minimum order quantity is 30kg. The price range is between 50-52 USD/kg and the delivery time is 15-20 days. The payment terms are T/T or L/C and the supply ability is 100000KG/MONTH. Packaging is provided in wooden boxes.

Customization:

Customized Inconel Alloy Services

  • Brand Name: KAIXIN
  • Model Number: Inconel 600
  • Place of Origin: China
  • Certification: ISO9001:2005
  • Minimum Order Quantity: 30kg
  • Price: 50-52 USD/kg
  • Packaging Details: Wooden Box
  • Delivery Time: 15-20 Days
  • Payment Terms: T/T L/C
  • Supply Ability: 100000KG/MONTH
  • Shape: Wire, Strip, Rod, Pipe, Plate
  • Executive Standard: ASTM
  • Delivery State: Sosoloid
  • Raw Materials: NI50-55%, CR17-21%, NB4.75-5.5%, MO2.8-3.3%
  • Application: Parts for Aero-engine, Nuclear Energy Industry and Petroleum Applications
  • Special Emphasis: Inconel 625 Tube, No. 6625, Alloy 625 Pipe

Support and Services:

Inconel Alloy provides technical support and service to its customers. Customers can contact the technical support team via phone, email or online chat. The team is available 24/7 to help with any queries that may arise. Additionally, the company provides online resources including technical documents, videos, tutorials and forums. All these resources can be accessed to provide customers with the information they need to get the most out of their Inconel Alloy products.

FAQ:

Q1: What is Inconel Alloy?
A1: Inconel Alloy is a nickel-chromium-based superalloy that has excellent corrosion and heat resistance. It is widely used in aerospace, chemical and petrochemical industries.
Q2: What is the brand name of Inconel Alloy?
A2: The brand name of Inconel Alloy is KAIXIN.
Q3: What is the model number of Inconel Alloy?
A3: The model number of Inconel Alloy is Inconel 600.
Q4: What is the minimum order quantity of Inconel Alloy?
A4: The minimum order quantity of Inconel Alloy is 30kg.
Q5: What is the price of Inconel Alloy?
A5: The price of Inconel Alloy is 50-52 USD/kg.


Product Tags:

600 Inconel Alloy

      

Nickel Based Deformed Superalloy

      

ASTM Standard Inconel Alloy

      
Cheap ASTM Standard Alloy 600 Inconel Alloy Nickel Based Deformed Superalloy And MO2.8-3.3% for sale

ASTM Standard Alloy 600 Inconel Alloy Nickel Based Deformed Superalloy And MO2.8-3.3% Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Danyang Kaixin Alloy Material Co., Ltd.
*Subject:
*Message:
Characters Remaining: (0/3000)